Rotary Kiln Size Sponge Iron Retention Time

Sponge iron composition manufacturing process lloy sponge iron making is a process in which iron ore lumps typically 5mm18mm size are tumbled with a selectgrade of ironcoking coal little dolomite inside an inclined rotary kiln and control busted in the presence of air for about 12 hours before the products are air cooled magnetically separated screened and size wise in finished product.